當前位置 -> 首頁新聞資訊哪些因素造成無錫環氧地坪漆表面黯淡無光? 發布時間:(2019/9/16)

哪些因素造成無錫環氧地坪漆表面黯淡無光?

標簽:混凝土密封固化劑 | 混凝土密封固化劑廠家

環氧地坪漆因為其優秀的裝飾效果,色彩多樣,表面光滑平整、光澤亮麗(啞光面除外),特別是環氧自流平地坪表面能達鏡面效果,一直深受人們的喜愛。但是有些消費者發現無錫環氧地坪漆施工后表面光澤度不夠、黯淡無光,嚴重影響環氧地坪漆的表面視覺效果。這是什么原因呢?又該如何預防呢?

Because of its excellent decorative effect, various colors, smooth surface, bright gloss (except matte surface), especially the mirror effect of the self-leveling epoxy floor paint, has been deeply loved by people. However, some consumers find that the surface gloss of epoxy floor paint is not enough and dull after construction, which seriously affects the surface visual effect of epoxy floor paint. What is the reason for this? And how to prevent it?

 環氧地坪漆表面暗淡無光的原因

Reasons for dull surface of epoxy floor paint:

1、因為貪圖便宜,選擇了環氧地坪漆價格相對較低卻質量有問題的材料,導致施工后的環氧地坪達不到預期的效果。

1. Because of the greed for cheapness, epoxy flooring paint has been chosen for materials with relatively low price but poor quality, resulting in the construction of epoxy flooring can not achieve the desired results.

2、環氧地坪漆材料使用時沒有按照廠家的要求加入了過量的稀釋劑,或者選擇的稀釋劑不配套,沸點低,揮發過快。

2. When using epoxy floor paint material, there is no excessive diluent added according to the requirements of the manufacturer, or the selected diluent is not matched, boiling point is low and volatilization is too fast.

3、在上一道涂層未完全干透就進行面漆的施工,導致環氧環氧地坪漆黯淡無光。

3. The application of topcoat before the last coat is completely dried leads to a dull epoxy floor paint.

4、基層地面沒有使用環氧地坪研磨機打磨平整,地面粗糙,導致環氧地坪漆施工后也不平整,光線折射導致涂膜表面光澤度不夠。

4. The base floor is not polished flat by using floor grinder, and the ground is rough, which results in the unevenness of epoxy floor paint after construction. The light refraction results in the insufficient gloss of the coating surface.

5、環氧地坪漆施工時環境溫度過高,過高的溫度會導致地坪漆起皺,影響表面的光澤度。

5. When epoxy floor paint is constructed, the ambient temperature is too high. Excessive temperature will cause wrinkling of the floor paint and affect the gloss of the surface.

6、環氧地坪漆施工現場環境濕度過大(相對濕度80%以上),導致環氧地坪漆漆膜吸收水分后泛白,失去光澤。

6. The environmental humidity of epoxy floor paint construction site is too high (the relative humidity is over 80%), which causes the epoxy floor paint film to become white after absorbing water and lose luster.


避免環氧地坪漆黯淡無光的方法

Method to avoid dull epoxy floor paint:

1、選擇正規地坪漆廠家生產的有質量保證的材料。

1. Choose materials with quality assurance produced by regular floor paint manufacturers.

2、嚴格按照地坪漆廠家的要求,添加環氧地坪漆配套的稀釋劑。

2. In strict accordance with the requirements of flooring paint manufacturers, add diluents for epoxy flooring paint.

3、面漆施工時一定要等待上一涂層完全干透。

3. When topcoat is applied, it must wait for the top coat to be completely dry.

4、環氧地坪漆施工前一定要用地坪研磨機將地面打磨平整,并將油污、雜物等清理干凈。

4. Before the construction of epoxy floor paint, the ground must be ground flat by a floor grinder, and the oil and sundries should be cleaned up.

5、環氧地坪漆最佳施工溫度是5-25攝氏度,施工時要避開高溫時段;

5. The optimum construction temperature of epoxy floor paint is 5-25 degrees Celsius. It is necessary to avoid high temperature during construction.

6、無錫環氧地坪漆施工時環境濕度不能高于80%。

6. The ambient humidity should not be higher than 80% during the construction of epoxy floor paint.

本站網址:http://www.www.jatrabd.com


來源:無錫環氧地坪公司  瀏覽次數:1064
相關閱讀:廠家對無錫環氧地坪翻新方法技巧經驗分享 | 無錫環氧地坪夏季施工為什么會出現色差? | 無錫環氧地坪漆的脫落原因與防范技巧
 
 
產品分類    
普通型環氧地坪 環氧玻璃鋼(FRP)地坪 丙烯酸地坪
環氧砂漿地坪 乙烯基酯重防腐地坪 EPPU聚合型工業地坪
環氧彩砂地坪 非金屬金屬耐磨地坪 停車場地坪
環氧自流平地坪 混凝土密封固化劑 環保型無毒防霉墻面
環氧防靜電地坪 自流平水泥地坪 有機硅丙烯酸室外防腐地坪


聯系我們
電 話:0510-88706248/13915319875
傳 真:0510-88706348
郵 箱:Yxdspeed@163.com
網 址:www.www.jatrabd.com
地 址:無錫市東亭錫滬東路11號
版權所有:無錫市思必德科技有限公司    網站關鍵詞:無錫環氧地坪  混凝土密封固化劑  蘇ICP備20046775號    技術支持:無錫易商科技    網站地圖
友情鏈接:梳理機 臺州討債公司 銼刀 金華討債公司 鹽城環氧地坪 武漢討債公司 無錫保潔公司 腳手架廠家 無錫環氧地坪
欧美自拍亚洲精品动图_欧美精品免费观看二区_97精品伊人久久大香线蕉_亚洲熟妇色xxxxx欧美老_人妻另类 专区 欧美 制服